MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Hybrid Plastics PK6U58.01 PEEK POSS® Flow Masterbatch
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: POSS® Flow masterbatches have shown success in reducing the melt viscosity of a variety of high temperature, difficult to process, thermoplastics. Hybrid Plastics offers such a solution for PEEK. PEEK POSS® Flow is a pellet masterbatch incorporating POSS® Flow in a PEEK carrier that can be used directly in the process or manufacturing stream. For injection molding applications, users will benefit from decreased molding pressures and increased flow for filling intricate and thin-walled parts. This leads to faster cycle times and less scrap. For extrusion applications, POSS® Flow will decrease screw torque, allowing for an increase in extrusion rate.

Typical addition levels are 10 to 20%. Adding 20% to a high molecular weight PEEK nearly doubled the MFI and decreased extrusion torque by 28%. At loading levels of up to 50%, there is no appreciable decrease in mechanical properties, including modulus, HDT and elongation to break. PEEK POSS® Flow is especially effective in filled systems. POSS coats and interacts with most fillers (glass, mineral, clay, etc.), improving dispersion and significantly decreasing melt viscosity.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.27 g/cc
Filler Content 10 - 50 %
Melt Flow 550 g/10 min
@Load 5.00 kg,
Temperature 380 °C
 
Descriptive Properties
ColorOpaque, light brown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHYBR037 / 88745

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.