MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Go Yen Chemical GY-1700 Wear Resistant Coupling Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Intro: GY-1700 series ,high performance additives, is developed by GO YEN CHEMICAL INDUSTRIAL CO. LTD. (GYC). It is a multifunctional additive which can apply to various kinds of synthetic resin and plastic industrial products. GY-1700 can apply to related resin industries to increase the chemical and physical functions, such as anti-wear, low surface tension, good anti-adhesion, weather resistance for improve the additional value to resin/plastic. And GY-1700 is non-toxic additive, so it has no influence on environment. Because GY-1700 series have various applications, it is beloved by synthetic plastic and leather companies in Europe, US, Japan, Korea.

Characteristic:

  • Offers a wide range of synthetic resin with excellent impact resistance and wear resistance.
  • With low surface tension and reduced viscosity
  • Enhance good abrasion resistance applied to PU and related products.
  • GY-1700 has great processing compatibility with resins.
  • Confer excellent tinting strength and weather resistance for all kinds of plastic.
  • Provide the products with fantastic smoothness and lubrication
  • GY-1700 is a non-toxic and environment-friendly additive without Teflon.
  • With good weather resistance and antioxidant capacity, suitable for outdoor synthetic products.
  • The recommended dosage of GY-1700 is 2%~7%.It can adjust according to different requirement.
Applications:
  • Various thermoplastic elastomers (TPU, TPE, SBS, SEBS…)
  • General plastic materials, such as PVC. PP. PE. PS construction board, and chassis.
  • Various rubber industry (CR, CSM, NR, SBR, SIR…etc)
  • PU synthetic leather, PVC, Nylon related products (special synthetic leather, various synthetic leather for sports ball, Industrial brake leather, Sofa leather, massage chair leather, automobile leather…etc)
  • Polycarbonate, nylon, polyacetal(POM), polysulfide, polyester
  • Resin, coating and surface anti-wear treatment for various industries.
  • Other specific applications

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/cc
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 1.0 %
 
Descriptive Properties
AppearanceWhite powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN319 / 266627

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.