MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Michelman® Coating X300™ AF Waterborne coating
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Waterborne coating demonstrating excellent water hold out

Usage: Coating X300™AF provides high levels of water resistance and good moisture resistance for kraft paper. Coating X300™ AF protects food products from excessive moisture, freezer burn, and sticking. When diluted for mill application, it is an economical sizing agent. Gluability with hot melt adhesives is excellent, but cold set gluing is not recommended.

Application data: Coating X300™ AF can be applied at the corrugator using a blade or rod coater.

Coating X300™ products are typically used for: Produce boxes that require protection from damp fields, wet fruit/vegetables and shipping ice; Meat, poultry and frozen food boxes that require release and protection from moisture within the box; Bakery products that require release and Building products that need protection in transit and on the job site

Food Contact Information when manufactured in the USA and Belgium:
FDA:
175.105: Components of adhesives.
176.170: Components of paper and paperboard in contact with aqueous and fatty foods.(Restricted)
176.180: Components of paper and paperboard in contact with dry foods.

When manufactured in Belgium product meets food contact regulations for:
Europe: Euro. Res. AP(2004)1 and Commission Regulation (EU) n° 10/2011
Germany: BfR Recommendation XIV (Restricted) and BfR Recommendation XXXVI (Restricted)

When manufactured in Singapore product meets food contact regulations for:
Europe: Euro. Res. AP(2004)1(Restricted)
Germany: BfR Recommendation XIV (Restricted) and BfR Recommendation XXXVI (Restricted)

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 - 1.00 g/cc
pH 9.3 - 10.3
Brookfield Viscosity 50 - 1000 cPSpindle # 3, rpm 60
Viscosity Measurement 10 - 45[sec], EZ cup, Cup # 3
 
Descriptive Properties
AppearanceWhite liquid
Solids TypeAcrylic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Gabriel Phenoxy™ PKHW-34 Polyhydroxylether, Emulsifier Free Waterborne Colloidal Dispersion
Evonik UNI-CAL® 866-1309 Colorant
Evonik COLORTREND® PLUS™ 802-5511 Universal Machine Colorant
Evonik COLORTREND® 888-1045 Universal Machine Colorant
Evonik COLORTREND® 817-2032 Universal Machine Colorant

WMICHEL004 / 134921

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.