MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
NOVA Chemicals NOVAPOL® LA-0219-A LDPE Foam Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes:

Homopolymer

Features:

  • Versatile multipurpose foam processing
  • Good foam-processing window
  • Suitable drawdown characteristics
  • Maintains foam dimensional stability
  • Achieves packaging-foam density

Additives:

  • Base resin

Applications:

  • Edge protection
  • Foam sheet and profile extrusion
  • Conventional and cross-linked foams
  • Specialty foams

Film properties are typical of blown film extruded at a blowup ratio of 2.5:1, but are dependent upon operating conditions.

United States: NOVAPOL LA-0219-A resin complies with the specifications contained in the U.S. Food and Drug Administration (FDA) regulation 21 CFR 177.1520 for olefin polymers, para. (c) 2.1, and may thus be used in the United States as an article or component of an article intended for use in contact with food. This resin is subject to the specific limitation that it may not be used in articles used for packing or holding food during cooking.

NOVA Chemicals polyethylene resins are biologically and chemically inert.

Information provided by NOVA Chemicals®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccASTM D 792
Thickness 38.0 microns
Melt Flow 1.67 g/10 minMelt Strength
Melt Index of Compound 2.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 10.0 MPaASTM D 882
Film Tensile Strength at Yield, TD 9.00 MPaASTM D 882
Tensile Strength, Yield 8.80 MPaASTM D 638
Film Elongation at Break, MD 350 %ASTM D 882
Film Elongation at Break, TD 550 %ASTM D 882
Elongation at Break 712 %ASTM D 638
Flexural Modulus, 1% Secant 296 MPaASTM D 790
Coefficient of Friction >= 0.60ASTM D 1894
Elmendorf Tear Strength MD 225 gASTM D 1922
Elmendorf Tear Strength TD 150 gASTM D 1922
Dart Drop Test 90.0 gF50; ASTM D 1709/A
Film Tensile Strength at Break, MD 18.0 MPaASTM D 882
Film Tensile Strength at Break, TD 16.0 MPaASTM D 882
1% Secant Modulus, MD 150 MPaASTM D 882
1% Secant Modulus, TD 175 MPaASTM D 882
 
Optical PropertiesOriginal ValueComments
Haze 12 %ASTM D 1003
Gloss 40 %@ 45°; ASTM D 2457
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
Low Friction Puncture (J/mm)45NOVA Chemicals test method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Armacell OleTex® BKJN 200 LDPE Foam
ExxonMobil Santoprene® 8271-55B100 Thermoplastic Elastomer
NOVA Chemicals DYLITE® F271C Expandable Polystyrene Resin
Vycom CELTEC MARINE™ Expanded Foam PVC Polyvinyl Chloride
St. Cloud Natural Zeolite (Clinoptilolite)

PNOVB019 / 194627

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.