MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexWeb® Aluminum Flex-Core® 5052/F40-0.0037 gauge Formable Aluminum Honeycomb
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: Description: HexWeb® Aluminum Flex-Core® honeycomb utilizes either 5052 or 5056 alloy foil material and is available in two cell sizes. Flex-Core® has unique cell configurations that significantly reduce anticlastic behavior and permit small radii of curvature without deformation of the cell walls or loss of mechanical properties.

Features

  • Commercially available aluminum honeycomb core specifically designed for formability
  • Retains mechanical properties in sharp curvatures
  • Offers cost savings for curved panels
  • Available in two cell sizes
Applications: HexWeb® Aluminum Flex-Core® has been developed by Hexcel to allow the designer and fabricator freedom in the utilization of honeycomb for components requiring simple and compound curvatures. Highly contoured sandwich panels such as leading edges and flaps, nacelles, fairings, doors and access covers, and other parabolic, spherical and cylindrical shapes are prime Flex-Core® candidates. Duplicate die model and control tooling for aerospace use are also examples of Flex-Core® applications. As with standard aluminum honeycomb, Flex-Core® provides controlled crush characteristics without rebound and thus curved energy absorption units become feasible and economical. HexWeb® CR-PAA outperforms standard AMS-C-7438 core in salt spray and crack propagation tests.

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0913 g/cc
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength >= 0.630 ksiBare
 >= 0.700 ksiStabilized
 0.935 ksiBare, Typical
 1.05 ksiStabilized, Typical
Compressive Modulus 290 ksiStabilized
Shear Modulus 23.0 ksiBeam, W Direction
 68.0 ksiBeam, L Direction
Shear Strength >= 0.170 ksiW Direction
 0.230 ksiW Direction, Typical
 >= 0.280 ksiL Direction
 0.400 ksiL Direction, Typical
 
Descriptive Properties
Crush Strength380 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NHECXB9201 / 322357

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.