MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Lupolen 1800P Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Lupolen 1800P is a low density polyethylene resin used in injection molding and other processing methods. It exhibits high flowability, and good softness, toughness and dimensional stability. Lupolen 1800 P is delivered in pellet form and is not additivated. Lupolen 1800P is used in applications such as compounding, toys, caps & closures, engineering parts, and sports and leisure equipment. Lupolen 1800P is not intended for use in medical and pharmaceutical applications. Applications: Caps & Closures, Sports, Leisure & Toys

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccISO 1183-1
Environmental Stress Crack Resistance >= 2.0 hourcond. B, 10% Arkopal N100; ASTM D1693
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 45ISO 868
Ball Indentation Hardness 12.0 MPaISO 2039-1
Tensile Strength, Yield 9.00 MPaISO 527-1,-2
Tensile Modulus 200 MPaISO 527-1,-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 105 °CISO 3146
Vicat Softening Point 82.0 °CA50N; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 230 °C
 
Descriptive Properties
Ball Indentation Hardness (MPa)H49/30
Processing MethodCompounding, Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Lupolen 1800U Polyethylene
LyondellBasell Lupolen 1800S Polyethylene

PEQT8525 / 220160

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.