MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Belsil® CM 7026 VP C26 – 28 Alkyl Methicone
Categories: Fluid; Polymer

Material Notes: BELSIL® CM 7026 VP is a high melting, white to cream colored, silicone wax that is resistant to hydrolysis and has a very high affinity to all kinds of substrates.

Application: The main applications of this silicone wax is in skin protection, skin care, sunscreens and decorative cosmetics. In skin care products, it improves the formulation efficiency and provides a soft, non-sticky skin feel. The BELSIL® CM 7026 VP forms an occlusive film, which reduces trans-epidermal water loss (TEWL). Its high substantivity, improved water resistance and moisturizing properties make this alkyl-functional silicone wax an indispensable component of sunscreen products and decorative cosmetics, such as lipsticks, mascara and make-up.

INCI name: C26 – 28 Alkyl Methicone

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 70.0 °C
 
Descriptive Properties
Appearancesolid wax
Colorwhite to cream colored
Solubility3-(4-Methylbenzyliden)-camphorinsoluble
 Avocado oil>10%
 Beeswax>10%
 BELSIL® DM 0.65insoluble
 BELSIL® DM 1 Plusinsoluble
 BELSIL® DM 100insoluble
 BELSIL® DMC 6031insoluble
 BELSIL® PDM 20insoluble
 BELSIL® SDM 5055insoluble
 C12-15 alkyl benzoates>10%
 Candelila wax1-10%
 Caprylic/Capric triglyceride>10%
 Castor oilinsoluble
 Decyl oleate>10%
 Ethylhexyl methoxycinnamateinsoluble
 Glycerolinsoluble
 Isocetyl isostearate>10%
 Isopropyl myristate>10%
 Isopropyl palmitate>10%
 Jojoba oil>10%
 Microcrystalline wax>10%
 Mineral oil (high-viscosity)>10%
 Mineral oil (low-viscosity)>10%
 Myristyl lactateinsoluble
 Octyl dodecanol1-10%
 Octyl salicylate>10%
 Oleyl alcohol>10%
 Oleyl oleate>10%
 Ozokerite wax>10%
 Propylene glycolinsoluble
 Tridecyl neopentanoateinsoluble
 Waterinsoluble
 Wheat germ oil1-10%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eagle Brass 7026 Copper Nickel, Annealed
Eagle Brass 7026 Copper Nickel, 1/4 Hard
Eagle Brass 7026 Copper Nickel, 1/2 Hard

PWACK9011 / 204540

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.