MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Chemours Krytox™ 240AB9H-1) PFPE Aerospace Grade Fluorinated Grease, Aerospace Grease Grade
Categories: Fluid; Lubricant; Perfluoropolyether (PFPE)

Material Notes: Many grades and special formulations of Krytox™ oils and greases offer superior performance characteristics and certifications for aerospace applications. They operate effectively in high vacuum and extreme temperatures, and are able to endure exposure to fuels, oxidizers, and radiation.

Features:

  • Unaffected lubricity and viscosity within a wide temperature range
  • Stable physical properties over time, including radiation resistance
  • Virtually unaffected by harsh environments and caustic chemicals
  • Resistant to vapor loss in a vacuum (e.g., during high-altitude orbit or deep space flight)
  • Long wear and low-energy consumption due to excellent friction-reducing characteristics
  • Compatible for use with most metals, elastomers, plastics, paints, and finishes,
  • Nontoxic, nonflammable, inert, and non-evaporative.

Information provided by Chemours Krytox

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.92 g/ccgrease
Volatiles 1.9 %
@Treatment Temp. 149 °C,
Time 79200 sec
wt% loss; ASTM D2595
 17.3 %
@Treatment Temp. 204 °C,
Time 79200 sec
wt% loss; ASTM D2595
 76.2 %
@Treatment Temp. 260 °C,
Time 79200 sec
wt% loss; ASTM D2595
Viscosity Measure 2.1 cSt
@Temperature 204 °C
base oil; ASTM D445
 10.5 cSt
@Temperature 99.0 °C
base oil; ASTM D445
 86 cSt
@Temperature 38.0 °C
base oil; ASTM D445
 240 cSt
@Temperature 20.0 °C
base oil; ASTM D445
Vapor Pressure 0.00000500 torr
@Temperature 38.0 °C
base oil; Knudsen
 0.0300 torr
@Temperature 260 °C
base oil; Knudsen
 
Mechanical PropertiesOriginal ValueComments
Penetration 265 - 29560 strokes; ASTM D217
Oil Separation 4.0 %
@Treatment Temp. 99.0 °C,
Time 108000 sec
wt% loss; ASTM D6184
 12 %
@Treatment Temp. 204 °C,
Time 108000 sec
wt% loss; ASTM D6184
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 232 °C
Minimum Service Temperature, Air -40.0 °C
Pour Point -40.0 °CASTM D97
 
Descriptive Properties
Liquid Oxygen ImpactPassASTM D2512, NASA MSFC 106B
Mechanical StabilityNo change from original grade10000 and 100000 strokes. ASTM D217
Oxidation Stability0 psig O2 pressure dropAfter 600 hr. 99°C. ASTM D942
TextureButtery

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WDUPJ811 / 253999

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.