System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Morgan Advanced Ceramics CIM Zirconia Technical Ceramic
Categories:
Ceramic
;
Oxide
;
Zirconium Oxide
Material Notes:
A very high purity zirconia-based material, partially stabilized with yttria.
Applications: Components for a range of medical, analytical and industrial applications.
information provided by Morgan Advanced Materials
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
>=
6.00
g/cc
Porosity
0.00 %
fully dense, nominal
Grain Size
0.20
µm
Mechanical Properties
Original Value
Comments
Hardness, Rockwell 45 N
87
Modulus of Elasticity
220
GPa
@Temperature 20.0 °C
Young's
Flexural Strength
<=
800
MPa
@Temperature 20.0 °C
4-point
Fracture Toughness
10.0
MPa-m½
Electrical Properties
Original Value
Comments
Volume Resistivity
<=
1.00e+10
ohm-cm
@Temperature 100 °C
Dielectric Constant
33
@Frequency 1e+10 Hz,
Temperature 20.0 °C
Thermal Properties
Original Value
Comments
CTE, linear
9.00
µm/m-°C
@Temperature 20.0 - 1000 °C
Specific Heat Capacity
0.610
J/g-°C
Thermal Conductivity
2.90
W/m-K
@Temperature 20.0 °C
Component Elements Properties
Original Value
Comments
ZrO2+Y2O3
99.9 %
includes HfO2
Descriptive Properties
Color
white
Thermal Shock Resistance (R1), delta T/C
400
Thermal Shock Resistance (R2), W/m
891
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
CeramTec ATZ Alumina Toughened Zirconia, Dental Grade
CoorsTek DuraSense™ Ceramic Alumina Toughened Zirconia
CeramTec MZ 111 Zirconia, ZrO2-Y2O3
Morgan Advanced Ceramics Nilcra® Zirconia 3Y-TZP Grade Y-TZP
Overview of materials for Nylon 12
CMORF8042 / 203519
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.