A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range of applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable. Key Features: - UL listed: file #QMFZ2.E80017, Plastics - Component; file #QMFZ8.E80017, Plastics Certified For Canada - Component.
- Although not NSF certified, this product has a Material Supplier Form on file with NSF to facilitate its evaluation for use in applications requiring NSF certification
- Excellent ozone resistance.
- EU and China RoHS compliant.
Applications: Uses:- Appliance Components
- Automotive Applications
- Automotive Under the Hood
- Consumer Applications
- Diaphrams
- Electrical Parts
- Living Hinges
- Tubing
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical |
EU 2003/11/EC; RoHS Compliant; UL QMFZ2; UL QMFZ8 |