MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Teknor Apex Tekbond® TB 2005 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, but also create a novel tactile and aesthetic experience. Tekbond® TPEs enable insert and 2-shot molding production of hybrid parts requiring distinctive functional and aesthetic performance criteria and marketing appeal, often at substantially reduced finished cost. Designer engineers have been selecting Tekbond® TPE to replace the more expensive and higher density TPUs. Tekbond® applications include hand held electronics and industrial diagnostic devices, lawn & garden and power tools.

Special Characteristic: Higher Hardness

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.02 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65
Tensile Strength 1300 psi
Elongation at Break 700 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Laripur® LPR 7560EG Thermoplastic Polyurethane
Teknor Apex Monprene® MP 1544 Thermoplastic Elastomer
Teknor Apex Monprene® MP 1644 Thermoplastic Elastomer
Teknor Apex Laripur® LPR 9060EF Thermoplastic Polyurethane
Teknor Apex Laripur® LPR 8860EG Thermoplastic Polyurethane

PTEKNO805 / 128986

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.