MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Gabriel VERSACURE™ RAC 9059 LC Phenalkamine Curing Agent
Categories: Other Engineering Material; Catalyst/Initiator

Material Notes: Industrial primers and floor coatings

Versacure® Phenalkamines contain amine, phenol, aromatic, and aliphatic structures, differentiating them from other polyamides and polyamine curing agents. They provide unique properties that give formulators a wide window to operate. To meet the most demanding needs, Versacure® Phenalkamines include products with a wide range of viscosities and reactivities.

Advantages:

  • Low temperature cure/year-round use
  • Excellent water and chemical resistance
  • Excellent adhesion
  • Flexibility
  • High solids formulations - VOC compliance

Information provided by Gabriel Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 500 - 1500 cP
 
Descriptive Properties
Amine Hydrogen Equivalent Weight95
Amine Value320-360[mg KOH/g]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGABR942 / 230643

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.