MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound DX96651 Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP LUBRICOMP DX96651 compound is based on Polycarbonate (PC) resin containing proprietary fillers. Added features of this grade include: Wear Resistant.

Features: Wear resistant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.23 g/ccASTM D792
 1.23 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.160 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0070 cm/cm24hrs; ASTM D955
 0.0073 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0070 cm/cm24hrs; ASTM D955
 0.0075 cm/cm24hrs; ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 46.0 MPaISO 527
 58.0 MPaASTM D638
Tensile Strength, Yield 48.0 MPaASTM D638
 55.0 MPaISO 527
Tensile Modulus 2200 MPa50 mm/min; ASTM D638
 2400 MPa1 mm/min; ISO 527
Flexural Strength 90.0 MPaISO 178
 93.0 MPaASTM D790
Flexural Modulus 2480 MPaASTM D790
 2600 MPaISO 178
Izod Impact Notched 101 JASTM D256
Izod Impact, Unnotched NBASTM D4812
Izod Impact, Notched (ISO) 9.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 137 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 41.0 Jpeak; ASTM D3763
Impact Test 128 JMultiaxial Impact; ISO 6603
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 175 - 250 VUL 746A
Hot Wire Ignition, HWI 60 - 120 sec
@Thickness >=3.00 mm
UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 65.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 65.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 66.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 V-2
@Thickness >=1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 305 - 315 °C
Zone 3 310 - 320 °C
Melt Temperature 300 - 315 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 120 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80762 / 288709

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.