Typical applications include (aerospace) vane plugs, fuel metering pins, spacer bushings, (bearings) ball blanks, race blanks, (valve seat inserts) diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous wear parts. Adhesive wear test data: P/M 0.10, Cast 0.24. Data provided by the manufacturer, Deloro Stellite Inc.Product of former Deloro Stellite Inc. |