MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Escorene® LL-3201 LLDPE/Hexene Premium High Strength 0.6 mil Film, Stiff  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Hexene, Film Grade

Material Notes: Data provided by the manufacturer, Exxon Chemical.

An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior properties along with the resin's good drawdown capability permit usage in many demanding packaging applications

Applications: Grocery sacks; Merchandise bags; Frozen food packaging; Heavy duty bags; Stretch film. Data for film properties below based on 0.6 mil film.

Key Words: Linear Low Density Polyethylene; Exxon Chemical Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.925 g/ccExxon Method
Thickness 0.600 mil
Melt Flow 0.80 g/10 minExxon Method
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 12.4 MPaASTM D882
Film Tensile Strength at Yield, TD 13.7 MPaASTM D882
Film Elongation at Break, MD 480 %ASTM D882
Film Elongation at Break, TD 730 %ASTM D882
Secant Modulus, MD 0.262 GPaASTM D882
Secant Modulus, TD 0.324 GPaASTM D882
Elmendorf Tear Strength MD 80 gASTM D1922
Elmendorf Tear Strength TD 640 gASTM D1922
Elmendorf Tear Strength, MD 133 g/milASTM D1922
Elmendorf Tear Strength, TD 1067 g/milASTM D1922
Dart Drop 133 g/milF50; ASTM D1709
Dart Drop Test 80.0 gF50; ASTM D-1709
Film Tensile Strength at Break, MD 66.2 MPaASTM D882
Film Tensile Strength at Break, TD 46.9 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 124 °CExxon Method
 
Optical PropertiesOriginal ValueComments
Haze 11 %ASTM D1003
Gloss 50 %45°, ASTM D-2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEXCGW / 37980

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.