System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Envalior Pocan® DP 7318 000000 PBT, 17% White Pigment
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), Unreinforced, Molded
Material Notes:
PBT, 17% white pigment, reduced warpage, high light-reflecting properties
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.50
g/cc
ISO 1183
Filler Content
17 %
White pigment
Linear Mold Shrinkage, Flow
0.019
cm/cm
Plaque 60 x 60 x 2mm; ISO 294-4
Linear Mold Shrinkage, Transverse
0.019
cm/cm
Plaque 60 x 60 x 2mm; ISO 294-4
Melt Flow
27
g/10 min
@Load 2.16 kg,
Temperature 260 °C
ISO 1133
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
57.0
MPa
5 mm/min; ISO 527-1,-2
Elongation at Break
10 %
5 mm/min; ISO 527-1,-2
Tensile Modulus
3400
MPa
1 mm/min; ISO 527-1,-2
Flexural Strain at Yield
6.0 %
2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)
<=
10.0
kJ/m²
@Temperature 23.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO)
10.0
kJ/m²
@Temperature 23.0 °C
ISO 180-1U
Charpy Impact Unnotched
125
kJ/m²
@Temperature 23.0 °C
ISO 179-1eU
Electrical Properties
Original Value
Comments
Comparative Tracking Index
600
V
Test solution A; IEC 60112
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
90.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow
90.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Melting Point
225
°C
10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi)
160
°C
Method Af; ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi)
190
°C
Method Bf; ISO 75-1,-2
Shrinkage, MD
0.20 %
@Treatment Temp. 120 °C,
Time 14400 sec
Flow Direction Post-Molding, Plaque 60 x 60 x 2mm; ISO 294-4
Shrinkage, TD
0.20 %
@Treatment Temp. 120 °C,
Time 14400 sec
Post-Molding, Plaque 60 x 60 x 2mm; ISO 294-4
Processing Properties
Original Value
Comments
Melt Temperature
260
°C
Plaque 60 x 60 x 2mm
Mold Temperature
80.0
°C
Plaque 60 x 60 x 2mm
Hold Pressure
60.0
MPa
Plaque 60 x 60 x 2mm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PLANW9042 / 208437
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.