MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Beologic Beobase 25 PP wood INJ132 GF Injection Molding
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Wood Filled

Material Notes: Main properties: visual natural fiber, high stiffness and good impact. Applications: industrial and consumer goods, furniture, non-food markets, automotive

Information provided by Beologic.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccISO 1183-1
Melt Flow 20.4 g/10 min
@Load 16.0 kg,
Temperature 230 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 44.4 MPaISO 527-1
Elongation at Break 3.4 %ISO 527-1
Tensile Modulus 3700 MPaISO 527-1
Flexural Modulus 3315 MPaISO 178
Charpy Impact Unnotched 23.5 kJ/m²ISO 179-1eU
Charpy Impact, Notched 4.50 kJ/m²ISO 179-1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 146 °CISO 75-1 (B)
Vicat Softening Point 113 °CB120; ISO 306
 
Descriptive Properties
Beologic Article Number2575050132
Carbon footprint (kg CO2 eq/kg)1.735PAS 2050
Natural fiber content (%)25
Renewable contentyes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBEOL9850 / 314136

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.