MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Park Aerospace Nelcote® F-555 Phenolic Prepreg, Glass Reinforced
Categories: Polymer; Thermoset; Phenolic

Material Notes: Nelcote® F-555 is a carbon-filled MIL-R-9299 phenolic resin optimized for coating Carbonized Rayon cloth. F-555 is used extensively in the manufacture of high temperature rocket nozzles, heat shields, and combustion chambers.

Key Features and Benefits:

  • Provides a combination of high-strength and ablative properties for demanding applications
  • Low thermal expansion
  • Good Tack and Drape properties

Applications/Qualifications:

  • Rocket Nozzles
  • Combustion Chambers
  • Heat Shields
  • Rocket Motor Throat Sections

Information provided by Park Electrochemical Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.08 g/cc18oz. woven roving form; ASTM D792
Volatiles 2.0 - 5.0 %
@Temperature 163 °C
5 min
Thickness 20.0 milper ply, 18oz. woven roving form
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 6818oz. woven roving form; ASTM D2583
Tensile Strength, Yield 51000 psi
@Temperature 23.9 °C
0° Direction, Dry; 18oz. Woven roving form; ASTM D638
Tensile Modulus 4200 ksi
@Temperature 23.9 °C
0° Direction, Dry; 18oz. Woven roving form; ASTM D638
Flexural Strength 33.2 ksi
@Temperature 23.9 °C
Dry; 18oz. Woven roving form; ASTM D790
Flexural Modulus 3400 ksi
@Temperature 23.9 °C
Dry; 18oz. Woven roving form; ASTM D790
Compressive Strength 22.0 ksi
@Temperature 23.9 °C
Dry; 18oz. Woven roving form; ASTM D695
Compressive Modulus 4700 ksi
@Temperature 23.9 °C
Dry; 18oz. Woven roving form; ASTM D695
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 4.44 °C
 
Descriptive Properties
Fabric Area Weight (g/m²)610
Prepreg Resin Content (%)28-34

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Lupolen 4532D High Density Polyethylene, Steel Pipe Coating Grade
Haveg 41NA Phenolic; Silicate Filled
Haveg 41N Phenolic; Silicate Reinforced Ablative Material
Evonik VESTAMID® NRG 4101 PA 12
Epoxy Technology EPO-TEK® 509FM-1 General Purpose Epoxy

PPARK057 / 89329

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.