MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Sandvik 22.8.3.L Welding wire
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Sandvik 22.8.3.L is a duplex stainless filler metal for welding duplex stainless steels such as Sandvik SAF 2205 and Sandvik SAF 2304. Corrosion resistance is equal to 904L in most applications. The grade can also be used for joining Sandvik SAF 2205 or Sandvik SAF 2304 to carbon steel.

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 240MIG and TIG
Tensile Strength, Ultimate 750 MPaMIG and TIG
 770 MPaSAW, FLUX 15W
Tensile Strength, Yield 600 MPa
@Strain 0.2 %
MIG and TIG
 650 MPa
@Strain 0.2 %
SAW, FLUX 15W
Elongation at Break 33 %SAW, FLUX 15W
 36 %MIG and TIG
Charpy Impact 85.0 J
@Temperature -20.0 °C
SAW, FLUX 15W
 90.0 J
@Temperature 20.0 °C
SAW, FLUX 15W
 100 J
@Temperature -20.0 °C
MIG and TIG
 160 J
@Temperature 20.0 °C
MIG and TIG
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.5 µm/m-°C
@Temperature 20.0 - 400 °C
Thermal Conductivity 16.0 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.020 %Filler metal
 <= 0.020 %MIG
 <= 0.020 %SAW
Chromium, Cr 22.5 %SAW
 23 %Filler metal
 23 %MIG
Manganese, Mn 1.2 %SAW
 1.5 %MIG
 1.6 %Filler metal
Nickel, Ni 0.14 %MIG
 0.15 %SAW
 0.16 %Filler metal
Phosphorus, P <= 0.020 %Filler metal
 <= 0.020 %MIG
 <= 0.025 %SAW
Silicon, Si 0.50 %Filler metal
 0.50 %MIG
 0.70 %SAW
Sulfur, S <= 0.015 %Filler metal
 <= 0.015 %MIG
 <= 0.015 %SAW

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Outokumpu 2205 Duplex Stainless Steel
AK Steel NITRONIC® 19-D Duplex Stainless Steel
Aluminum, Al
Carlson 2205 (UNS S31803) Duplex Stainless Steel
Astralloy 4800® Wear Resistant Steel

NSANDV5114 / 199678

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.