ELKONIUM® 63 alloy contains small amounts of magnesium and nickel. It is recommended for low voltage, vibrating contact DC applications for minimizing metal transfer. It is used in automobile voltage regulators and electrical gauges. In a heat-treated condition the material is CMW D63X alloy, a high strength material used for contact spring arms.Information provided by NAECO, LLC. |