MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Owens Corning Glass Fiber Reinforced Polyester (PET), 30 wt.% glass
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 30% Glass Reinforced

Material Notes: Thermoplastic Polyesters are resistant to most organic solvents, weak acids and alkalis. They are not recommended with strong acids and alkalis or for prolonged use in hot water. Data provided by the manufacturer, Owens Corning.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.56 g/ccASTM D792
Water Absorption 0.050 %24 hrs.; ASTM D570
Linear Mold Shrinkage 0.0030 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Tensile Strength, Ultimate 140 MPaASTM D638
Elongation at Break 6.6 %ASTM D638
Modulus of Elasticity 9.00 GPaASTM D638
Flexural Strength 220 MPaASTM D790
Flexural Modulus 8.62 GPaASTM D790
Compressive Strength 170 MPaASTM D695
Izod Impact, Notched 0.960 J/cm
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.6
@Frequency 60 Hz
ASTM D150
Dielectric Strength 520 V/milASTM D149
Arc Resistance 90 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kingfa PET-G30 30% Glass Fiber Reinforced PET
Cheng Yu Plastic E2325 Flame Retardant PET, 25% Glass Fiber
Adamas Rixon U PEEK, Unreinforced
EMS-Grivory Grilamid® LV-50H FWA black 9225 PA12-GF50
EMS-Grivory Grilamid® LBV-50H FWA nat PA12-GF50

POC022 / 55600

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.