Phenolic molding compound, inorganically filled, glass fiber reinforced, elastomer modified, galvanizable, heat resistant, good media resistance, high dimensional stability at raised temperature, high mechanical strength. Applications: Thermally and mechanically highly stressed automotive parts, solenoid switch caps, electrical motor end shields. |