System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
LyondellBasell Ultrathene UE650028 Ethylene Vinyl Acetate Copolymer (EVA), Blow Molding Grade
Categories:
Polymer
;
Film
;
Thermoplastic
;
Ethylene Vinyl Acetate
;
Ethylene Vinyl Acetate Copolymer (EVA), Blow MoldingGrade
Material Notes:
Ultrathene UE650028 is an EVA copolymer with excellent flexibility and low temperature properties. Applications: Foamed Sheet, Soft Profile & Sheets
Information provided by LyondellBasell.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.931
g/cc
ASTM D1505
Vinyl Acetate Content
12 %
LYB Method
Melt Flow
3.0
g/10 min
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Shore D
44
ASTM D 2240
Tensile Strength, Yield
14.5
MPa
ASTM D638
Elongation at Break
1100 %
ASTM D 638
Tensile Modulus
127
MPa
1% secant; ASTM D638
Thermal Properties
Original Value
Comments
Melting Point
93.0
°C
DSC; LYB Method
Vicat Softening Point
69.0
°C
ASTM D1525
Brittleness Temperature
<=
-76.0
°C
ASTM D746
Descriptive Properties
Processing Method
Blown Film, Cast Film, Sheet and Profile Extrusion
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Celanese Ateva® 1081G Medical Grade EVA
Tisan TISETILEN® Flame Retardant (V0) Polyethylene
Celanese Ateva® 2606A EVA polymer for adhesives, automotive, compounds and molding
Braskem TN2020 EVA General Film Copolymer
Bayport Polymers Baystar™ L425 HDPE Film
PEQT8585 / 220220
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.