MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC XENOY™ 1731 PC+PBT (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccASTM D792
 1.22 g/ccASTM D792
Density 1.22 g/ccISO 1183
Water Absorption 0.28 %23°C/sat; ISO 62
Moisture Absorption 0.0800 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 8.0 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ISO 1133
 9.6 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 56.0 MPa50 mm/min; ASTM D638
 58.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 60.0 MPa50 mm/min; ISO 527
 61.0 MPa50 mm/min; ASTM D638
Elongation at Break 90 %50 mm/min; ISO 527
 100 %50 mm/min; ASTM D638
Elongation at Yield 5.0 %50 mm/min; ASTM D638
 5.0 %50 mm/min; ISO 527
Tensile Modulus 2330 MPa1mm/min; ISO 527
 2370 MPa5 mm/min; ASTM D638
Flexural Yield Strength 93.0 MPa1.3 mm/min, 50 mm span; ASTM D790
 93.0 MPa2 mm/min; ISO 178
Flexural Modulus 2210 MPa2 mm/min; ISO 178
 2340 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 667 J/mASTM D256
 106 J/m
@Temperature -30.0 °C
ASTM D256
 160 J/m
@Thickness 6.40 mm
ASTM D256
Izod Impact, Notched (ISO) 59.0 kJ/m²80*10*4; ISO 180/1A
 16.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 65.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 61.0 JASTM D3763
 61.0 J
@Temperature -30.0 °C
ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Arc Resistance 120 - 180 secASTM D495
Comparative Tracking Index 250 - 400 VUL 746A
Hot Wire Ignition, HWI 30 - 60 secUL 746A
High Amp Arc Ignition, HAI >= 120 arcsUL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 77.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 77.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 82.8 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
CTE, linear, Transverse to Flow 75.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 75.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 93.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 107 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 125 °CRate B/50; ASTM D1525
 127 °CRate B/50; ISO 306
 130 °CRate B/120; ISO 306
UL RTI, Electrical 75.0 °CUL 746B
UL RTI, Mechanical with Impact 75.0 °CUL 746B
UL RTI, Mechanical without Impact 75.0 °CUL 746B
Flammability, UL94 HB
@Thickness 1.49 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 255 - 270 °CInjection Molding
Zone 1 245 - 265 °C
Zone 2 250 - 270 °C
Zone 3 255 - 275 °C
Melt Temperature 260 - 275 °C
Mold Temperature 65.0 - 90.0 °C
Drying Temperature 110 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 50 - 80 %
Vent Depth 0.00130 - 0.00200 cm
Screw Speed 50 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10811 / 244278

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.