MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Total Finathene® 3802N Natural HDPE pipe grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Applications: Natural gas distribution, extruded pipes, molded fittings, pipe coating, pipe lining

Information provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.939 g/ccASTM D 792
High Load Melt Index 20 g/10 min
@Load 21.6 kg
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
PENT >= 5000 hourASTM F 1473
Hardness, Shore D 65ASTM D 2240
Tensile Strength at Break 4000 psiASTM D 638 type IV
Tensile Strength, Yield >= 2600 psiASTM D 638 type IV
Elongation at Break >= 700 %ASTM D 638 type IV
Flexural Modulus 102000 psiASTM D 790
Hydrostatic Design Basis 1250 psi
@Temperature 23.0 °C
ASTM D 2837
 
Thermal PropertiesOriginal ValueComments
CTE, linear 216 µm/m-°C
@Temperature 20.0 °C
ASTM D 696
Melting Point 259 °FASTM D3417
Vicat Softening Point 260 °FISO 306

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Alathon® L5332CP High Density Polyethylene
A. Schulman LP552-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
LyondellBasell Hostalen CRP 100 RESIST CR orange High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Hostalen CRP 100 ORANGE High Density Polyethylene (HDPE), Pipe Grade
LyondellBasell Alathon® H5520 High Density Polyethylene

PFINAP112 / 38695

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.