MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro DESMODUR® TT194 + BAYTEC® XL 2190, 76 D Polyurethane, TDI- PTMEG
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes:

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.650 g/ccBAYTEC® XL 2190
 1.09 g/ccDESMODUR® TT194
 1.14 g/cc
Viscosity 440 cPDESMODUR® TT194
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 76DIN 53505
 69
@Temperature 80.0 °C
DIN 53505
 80
@Temperature -5.00 °C
DIN 53505
Tensile Strength at Break 54.0 MPaDIN 53504
Tensile Stress at Strain 39.0 MPa
@Strain 10 %
DIN 53504
Elongation at Break 175 %DIN 53504
100% Modulus 0.0430 GPa
@Strain 100 %
DIN 53504
Resilience 46[%]; DIN 53512
Tear Strength 113 kN/mwith nick; ISO 34-1
 218 kN/mwithout nick; ISO 34-1
Abrasion 50[mm3]; ISO 4649
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 °CDESMODUR® TT194
 110 °CBAYTEC® XL 2190
Mold Temperature 110 °C
Pot Life 0.583 min
 
Descriptive Properties
AppearanceliquidDESMODUR® TT194
 solidBAYTEC® XL 2190
Content100Parts by weight of prepolymer
 38.3Parts by weight of BAYTEC® XL 2190
 9.2-9.6%NCO, DESMODUR® TT194

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro DESMODUR® TTG528 + MOCA Polyurethane, TDI- Ether
Covestro DESMODUR® TTX131 + MOCA, 85 A Polyurethane, TDI- PTMEG
Covestro DESMODUR® TTX142L + MOCA, 90 A Polyurethane, TDI- PTMEG
Covestro DESMODUR® TTX146 + MOCA, 90 A Polyurethane, TDI- PTMEG
Covestro DESMODUR® TT163 + BAYTEC® XL 1705, 93 A Polyurethane, TDI- PTMEG

PCOVEST0662 / 202445

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.