MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound RP004 Polyamide 66 (Nylon 66) (Asia)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: LNP LUBRICOMP RP004 compound is based on Nylon 6/6 resin containing 20% PTFE/silicone. Added features of this grade include: Wear Resistant.

Features: Wear resistant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccASTM D792
 1.24 g/ccISO 1183
Moisture Absorption 0.800 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.019 cm/cm24hrs; ASTM D955
 0.019 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.019 cm/cm24hrs; ASTM D955
 0.019 cm/cm24hrs; ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPaASTM D638
 63.0 MPaISO 527
Tensile Strength, Yield 63.0 MPaISO 527
Elongation at Break 22.5 %ASTM D638
 26.6 %ISO 527
Elongation at Yield 22 %ASTM D638
 26 %ISO 527
Tensile Modulus 2730 MPa1 mm/min; ISO 527
 2750 MPa50 mm/min; ASTM D638
Flexural Strength 82.0 MPaISO 178
Flexural Modulus 2000 MPaISO 178
 2060 MPaASTM D790
Izod Impact Notched 53.0 JASTM D256
Izod Impact, Unnotched 347 J/mASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 88.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 6.00 Jpeak; ASTM D3763
Impact Test 1.00 JMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.19ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.040ASTM D3702 Modified: Manual
K (wear) Factor 3.00 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 82.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 84.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 93.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 94.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 200 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 237 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 63.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 65.0 °CUL 746B
UL RTI, Mechanical with Impact 65.0 °CUL 746B
UL RTI, Mechanical without Impact 65.0 °CUL 746B
Flammability, UL94 HB
@Thickness 0.750 mm
UL 94

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81037 / 288984

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.