DuraGrip® DGR6165TR is a translucent thermoplastic elastomer (TPE) formulated for excellent elastic properties and enhanced adhesion to engineered thermoplastics using insert molding, co-injection molding and co-extrusion processes. DGR6165TR bonds tenaciously to polycarbonate, polycarbonate alloys, ABS, ASA, acrylics, and cellulosic materials. It will also bond to various nylons and PET. DGR6165TR is hygroscopic and drying is recommended at 150F for 3 to 4 hours to ensure optimum aesthetics, properties and adhesion. Information provided by Advanced Polymer Alloys Former product line of Advanced Polymer Alloys (APA), acquired by A. Schulman in 2014. |