Product Description: LD 653 is an easy flowing LDPE grade with medium stiffness and good toughness. Availability: Africa & Middle East and Europe Additive: - Antiblock: No
- Slip: No
- Thermal Stabilizer: No
Applications: - Caps
- Closures
- Compounding
- Food Packaging Containers
- Houseware Articles
- Injection Molding
- Masterbatch Base Resin
- Toys
- Tough Medium Sized Molding
Information provided by ExxonMobil |