MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Leaded Red Brass, Copper Alloy, UNS C32000, H04 Temper, Wire
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Temper: Hard

Fabrication Properties: Excellent Suitability – Soldering; Good Suitability – Capacity for Being Cold Worked, Brazing; Fair Suitability – Butt Weld; Poor Suitability – Capacity for Being Hot Formed

Common Fabrication Processes: Drilling; Knurling; Machining; Roll Threading

Typical Uses: Hardware; Locknuts; Bushings; Caps; Couplings; Pipe Plugs; Regulators; Screw Machine Parts; Plumbers' Brass Goods; Plumbing Fittings

Applicable Specifications: Bar – ASTM B140/B140M; Rod – ASTM B140/B140M; Shapes – ASTM B140/B140M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.316 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 72.0 ksi
Tensile Strength, Yield 56.0 ksi0.5% Ext
Elongation at Break 4.0 %
Tensile Modulus 17000 ksi
Modulus of Rigidity 6400 ksi
Poissons Ratio 0.33Calculated
Machinability 90 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000480 ohm-cm36% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.4 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.0900 BTU/lb-°F
Thermal Conductivity 90.0 BTU-in/hr-ft²-°F
Melting Point 1820 - 1875 °F
Solidus 1820 °F
Liquidus 1875 °F
Annealing Point 800 - 1200 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 83.5 - 86.5 %
Iron, Fe <= 0.10 %
Lead, Pb 1.5 - 2.2 %
Nickel, Ni <= 0.25 %
Zinc, Zn 11.1 - 15 %As Balance

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC32000x4 / 291858

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.