Product Description: Mackamine CS is a pure grade of cocamine oxide that provides excellent foam boosting and foam stability. Mackamine CS is compatible with most surfactants and because there are no amide or ester groups, Mackamine CS will not hydrolyze in acid systems. Mackamine CS is also stable in highly alkaline products. This grade of cocamine oxide exhibits a particularly low level of free amine. Chemical Name: Cocamine Oxide CAS No.: 61788-90-7 EINECS: 263-016-9 Information provided by Solvay. Verdant Specialty Solutions was created through the purchase of Solvay's amphoteric and secondary surfactants business |