MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CMW® ELKALOY D Copper Alloy, Aluminum Bronze  (discontinued **)
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: ELKALOY® D alloys are aluminum bronze type casting alloys. The sequence, ELKALOY® D, D110, D120, D130 materials represents increasing hardness and abrasion resistance but reduced electrical and thermal conductivity and ductility. In the ELKALOY® D alloy impurities (including iron) are kept low to obtain maximum electrical thermal conductivity.

ELKALOY® D material is recommended for certain flash welding operations, particularly for cold rolled steel and stainless set. The entire die is made from ELKALOY® D material. ELKALOY® D material is also used as a backing on barrel welding dies, faced with either CMW® 73 or ELKONITE® materials. The material may be used as an inexpensive current carrying member for welders or welding jigs, fixtures, or dies where high electrical conductivity is not of prime importance. Typical examples of welder arms, knees, platens and die and fixture bases.

Information provided by CMW Inc.

1

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.60 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 75
Tensile Strength, Ultimate 438 MPa
Tensile Strength, Yield 207 MPa
Elongation at Break 8.0 %
Reduction of Area 8.0 %
Modulus of Elasticity 103 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000960 ohm-cm18 % IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 18.0 µm/m-°C
@Temperature 100 °C
Thermal Conductivity 67.0 W/m-K
Melting Point 1025 - 1060 °C
Solidus 1025 °C
Liquidus 1060 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 10 %
Beryllium, Be 0.50 %
Co + Ni 1.5 - 2.55 %
Copper, Cu 86.95 - 88 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CMW® ELKALOY D120 Copper Alloy, Aluminum Bronze
CMW® ELKALOY D130 Copper Alloy, Aluminum Bronze
Bohler-Uddeholm BeCu Alloy 172 Mold Material
Brush Wellman Beryllium Copper Alloy 165 Strip; 1/2H (TD02) Temper (UNS C17000)
Cadi MOLD-MOR™ 3

NCMW072 / 15885

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.