MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Pyro-Bloc® EES System ZR Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: The Pyro-Bloc Electric Element Support (EES) System is a complete engineered package which includes Pyro Bloc Y modules, heating elements, hanging systems, and detailed drawings, that are a cost-effective method of hanging electric heating elements from Pyro-Bloc modules. EES system was patented over 20 years ago on the pre-embedded tubes, located within a ceramic fiber module, and the supporting hooks and washers. Applications: The type of furnace plays an important role in element orientation and manner of installation. For example, a bell furnace that is constantly moved would be designed much differently than a stationary pit furnace. Other furnaces requiring special consideration include car bottoms, tip-ups, and furnaces that see vibration, such as from roller rails.

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.160 g/cc
 0.192 g/cc
 0.240 g/cc
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0700 W/m-K
@Temperature 260 °C
at 10 kg/m3; ASTM C201
 0.0700 W/m-K
@Temperature 260 °C
at 12kg/m3; ASTM C201
 0.0700 W/m-K
@Temperature 260 °C
at 15 kg/m3; ASTM C201
 0.120 W/m-K
@Temperature 538 °C
at 15 kg/m3; ASTM C201
 0.140 W/m-K
@Temperature 538 °C
at 12kg/m3; ASTM C201
 0.150 W/m-K
@Temperature 538 °C
at 10 kg/m3; ASTM C201
 0.210 W/m-K
@Temperature 816 °C
at 15 kg/m3; ASTM C201
 0.240 W/m-K
@Temperature 816 °C
at 12kg/m3; ASTM C201
 0.260 W/m-K
@Temperature 816 °C
at 10 kg/m3; ASTM C201
 0.310 W/m-K
@Temperature 1093 °C
at 15 kg/m3; ASTM C201
 0.350 W/m-K
@Temperature 1093 °C
at 12kg/m3; ASTM C201
 0.390 W/m-K
@Temperature 1093 °C
at 10 kg/m3; ASTM C201
Melting Point 1760 °C
Maximum Service Temperature, Air 1343 °CContinuous Use
 1427 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 37.5 %
SiO2 47 %
ZrO2 15.5 %
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF70127 / 203425

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.