MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bostik Ultra-Set® Singlestep2™ Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: Description: Ultra-Set® SingleStep2™ is a high performance adhesive, moisture control, and sound reduction membrane all in one. Bostik’s breakthrough AXIOS® Tri-Linking™ Polymer Technology used in this formulation maintains the superior long term durability, moisture control and sound abatement properties of high end urethane adhesives. However, it is easier to spread and clean off of prefinished flooring before and after cure. This adhesive contains 1% recycled rubber material, has zero VOC’s (as calculated per SCAQMD Rule 1168) and does NOT contain any water. Ultra- Set® SingleStep2™ comes with Bostik’s BLOCKADE® antimicrobial protection, which inhibits the growth of bacteria, mold or mildew on the surface of the cured membrane. The cured membrane resists stains caused by mold..

Key Features:

  • Easy clean before and after cure
  • Lifetime warranty for unlimited moisture vapor protection
  • Superior sound dampening performance

Information provided by Bostik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 14.25 lb/gal
Volatile Organic Compounds (VOC) Content 0.00 g/lSCAQMD Rule #1168
Water Vapor Transmission <= 0.400 g/m²/dayASTM E96
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break >= 100 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 150 °F
Minimum Service Temperature, Air -40.0 °F
Flash Point >= 200 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 50.0 - 100 °FApplication
Cure Time 8.00 - 12.0 hourLight foot traffic
 12.0 - 24.0 hourNormal foot traffic
 
Descriptive Properties
ColorBeige w/ black specks

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBOSTK032 / 191568

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.