MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
CMT Materials CTB 44 Composite Toolboard High Temperature
Categories: Polymer; Thermoset; Epoxy

Material Notes: CTB-44 is manufactured by CMT Materials for a wide variety of vacuum forming applications. It is suitable for use up to 2500F (1210C). CTB-44 utilizes a copolymer base material and smaller cell structure than most boards, providing improved mechanical properties and a smoother surface finish.
  • Excellent machinability
  • Superior edge definition
  • Good dimensional stability
  • Outstanding surface finish
Applications: CTB-44 is an excellent choice for constructing forming tools, master models, fixturing and other heat resistant applications. It may also be used for composite fabrication in pre-preg and autoclave cure, wet lay-up, vacuum infusion and other composite processes.

Information Provided by CMT Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 44.0 lb/ft³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80
Flexural Strength 6470 psi
Flexural Modulus 334 ksi
Compressive Strength 8010 psi
Compressive Modulus 290 ksi
 
Thermal PropertiesOriginal ValueComments
CTE, linear 22.0 µin/in-°F
 
Descriptive Properties
ColorBlue Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCMT012 / 93147

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.