MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ Copolymer EXL1330 Polycarbonate (PC) (Asia)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in combination with medium flow characteristics and excellent processability with opportunities for shorter IM cycle times compared to standard PC. LEXAN EXL1330 resin is a general purpose product available in a wide range of opaque colors and is an excellent candidate for a broad range of applications.

Features: High Impact Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccASTM D792
Density 1.18 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.0200 %Sheet Extrusion
 0.150 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.35 %ISO 62-1
Viscosity 9.0 cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 90.0 MPaH358/30; ISO 2039-1
Tensile Strength at Break 56.0 MPa50 mm/min; ISO 527
 61.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 55.0 MPa50 mm/min; ISO 527
 58.0 MPa50 mm/min; ASTM D638
Elongation at Break >= 100 %50 mm/min; ISO 527
 130 %50 mm/min; ASTM D638
Elongation at Yield 5.0 %50 mm/min; ISO 527
 6.0 %50 mm/min; ASTM D638
Tensile Modulus 2100 MPa50 mm/min; ASTM D638
 2100 MPa1 mm/min; ISO 527
Flexural Strength 85.0 MPayield, 2 mm/min; ISO 178
 88.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2060 MPa1.3 mm/min, 50 mm span; ASTM D790
 2100 MPa2 mm/min; ISO 178
Izod Impact Notched 801 JASTM D256
 587 J
@Temperature -50.0 °C
ASTM D256
 680 J
@Temperature -30.0 °C
ASTM D256
 640 J
@Thickness 6.40 mm
ASTM D256
Izod Impact, Notched 1068 J/mdouble-gated; SABIC method
Izod Impact, Notched (ISO) 70.0 kJ/m²80*10*3; ISO 180/1A
 55.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 75.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 60.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 52.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 175 - 250 VUL 746A
Hot Wire Ignition, HWI >= 120 sec
@Thickness >=0.800 mm
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness >=0.800 mm
UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 66.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 72.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 66.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 72.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 136 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 134 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
 120 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 124 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 143 °CRate B/50; ISO 306
 143 °CRate B/50; ASTM D1525
 145 °CRate B/120; ISO 306
UL RTI, Electrical 125 °CUL 746B
UL RTI, Mechanical with Impact 115 °CUL 746B
UL RTI, Mechanical without Impact 125 °CUL 746B
Flammability, UL94 HB
@Thickness >=0.800 mm
UL 94
Oxygen Index 35 %ISO 4589
Glow Wire Ignition Temperature 875 °C
@Thickness 0.800 mm
IEC 60695-2-13
 875 °C
@Thickness 1.00 mm
IEC 60695-2-13
 875 °C
@Thickness 1.50 mm
IEC 60695-2-13
 875 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 850 °C
@Thickness 0.800 mm
IEC 60695-2-12
 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 290 - 310 °C
Zone 1 250 - 290 °CSheet Extrusion
Zone 2 245 - 270 °CSheet Extrusion
 280 - 305 °C
Zone 3 225 - 255 °CSheet Extrusion
 295 - 315 °C
Adapter Temperature 225 - 255 °CSheet Extrusion
Die Temperature 240 - 260 °CSheet Extrusion
Melt Temperature 245 - 260 °CSheet Extrusion
 295 - 315 °CInjection Molding
Mold Temperature 70.0 - 95.0 °C
Roll Temperature 75.0 - 115 °CRoll Stack Temp - Top
 80.0 - 125 °CRoll Stack Temp - Middle
 120 - 145 °CRoll Stack Temp - Bottom
Drying Temperature 110 - 120 °CSheet Extrusion
 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 3.00 - 4.00 hourSheet Extrusion
 48.0 hourCumulative; Sheet Extrusion
 48.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80149 / 288096

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.