MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kostat BK-STAT P048BK PP Compound
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanliness requirements in comparison to other materials based on Hygroscopic Antistats, Inherently Conductive Polymer Coating, or Conductive Fillers such as carbon fibers and carbon blacks.

BK-STAT Compounds exhibit superior property and processing characteristics compared with other competitive IDP based compounds.

Special Features:

  • Superior Permanent Static Dissipation
  • Excellent Wear Resistance
  • Humidity Insensitivity
  • Exceptionally High Impact Resistance
  • No Particle Generation
  • Excellent Processibility

Applications:

  • Semiconductor Packaging
  • LCD Packaging
  • Electrical & Electronics
  • Medical Devices
  • Storage Disks
  • Appliances
  • Consumer Goods
  • Clean Room Accessories

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.920 g/ccASTM D792
Linear Mold Shrinkage 0.015 - 0.020 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 20.0 MPaASTM D638
Flexural Strength 20.0 MPaASTM D790
Flexural Modulus 0.880 GPaASTM D790
Izod Impact, Notched 190 J/mASTM D256
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+9 - 1.00e+11 ohmASTM D257
Static Decay <= 0.50 sec5kV to 50V; FTMS 101C
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Drying Temperature 60.0 - 70.0 °C
Dry Time 3 - 4 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Zylog Hipolyene® 1046 IFL Thermoplastic Polyolefin & PP Compound
Vibrantz Technologies EG 2807 Metal Sealing
Titanium Dioxide, Rutile
Titanium Beta C (Ti-3Al-8V-6Cr-4Mo-4Zr ST 815°C, Aged 510°C
Titanium (II) Bromide, TiBr2

PKOSTAT01 / 49036

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.