MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Lavergne VYPET VNT 840 HY PET 40% Glass-Mineral Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Glass/Mineral Reinforced

Material Notes: Vypet VNT 840 HY is a 40% glass/mineral reinforced PET high strength injection molding compound with improved hydrolysis stability designed for electrical and structural applications, with High Dielectric Strength

Features: High temperature performance; Excellent strength & high stiffness; Excellent dimensional stability; Better hydrolysis stability

Typical Applications: Electric motors; Brackets; Connectors

Information provided by Bieglo Gmbh for Lavergne Performance Compounds

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.61 g/ccISO 1183
Water Absorption 0.060 %
@Temperature 23.0 °C
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm
@Thickness 3.20 mm
3.2x7.6x12.6mm; ASTM D955
Linear Mold Shrinkage, Transverse 0.010 cm/cm
@Thickness 3.20 mm
3.2x7.6x12.6mm; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 109ASTM D785
Tensile Strength at Break 150 MPa5 mm/min; ISO 527
Flexural Strength 236 MPa2 mm/min; ISO 178
Flexural Modulus 10479 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²ISO 180
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.65e+16 ohm-cmASTM D257
Dielectric Constant 3.8
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 28.4 kV/mm
@Thickness 1.60 mm,
Temperature 23.0 °C
500 V/s in oil; ASTM D149
Dissipation Factor 0.0080
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ASTM E831
CTE, linear, Transverse to Flow 30.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ASTM E831
Melting Point 246 °C
Deflection Temperature at 1.8 MPa (264 psi) 225 °CISO 75
Flammability, UL94 HB
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Feed Temperature 260 - 270 °C
Middle Barrel Temperature 265 - 275 °C
Front Barrel Temperature 270 - 295 °C
Nozzle Temperature 275 - 300 °C
Melt Temperature 275 - 300 °C
Mold Temperature 75.0 - 120 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lavergne VYPET VNT 840 PET 40% Glass-Mineral Reinforced
E-Polymers SEPAZ® C130M 30% Mineral Reinforced LCP Resin

PLAVER929 / 150656

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.