MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ATI Wah Chang Nb/Nb Alloy Nb-I ZR
Categories: Metal; Nonferrous Metal; Niobium Alloy

Material Notes: Improved creep strength versus pure niobium. Replacement for pure niobium in applications requiring the chemical resistance of niobium and a material with high melting temperature.

Information provided by ATI Wah Chang

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.310 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 68.98 GPa
@Temperature 23.0 °C
Charpy Impact 155 ft-lb
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 290.4 BTU-in/hr-ft²-°F
Melting Point 2400 - 2420 °C
Solidus 2400 °C
Liquidus 2420 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.103
@Temperature 500 °C
Total Hemispherical
 0.11
@Temperature 600 °C
Total Hemispherical
 0.117
@Temperature 700 °C
Total Hemispherical
 0.13
@Temperature 800 °C
Total Hemispherical
 0.142
@Temperature 900 °C
Total Hemispherical
 0.154
@Temperature 100 °C
Total Hemispherical
 0.167
@Temperature 1100 °C
Total Hemispherical
 0.179
@Temperature 1200 °C
Total Hemispherical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Goodfellow Niobium 56/Titanium 44 Alloy
ATI Wah Chang Nb/Nb Alloy C-103
Elmet-Starck 2602 Molybdenum Powder Metallurgy Alloy ODS Mo-La
Niobium, Nb; High Purity
Niobium, Nb; Soft

NATIWC03 / 15058

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.