MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parker Chomerics SOFT-SHIELD® 5000 Low Closure Force EMI Gasket
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: Description: SOFT-SHIELD® 5000 Series EMI gaskets are designed to meet the stringent shielding and mechanical performance requirements of today’s commercial electronic enclosures, medical electronics, factory automation equipment, reprographics and grounding applications. Each gasket consists of an electrically conductive fabric jacket over a highly compressible urethane foam core. The nickel-plated, woven nylon rip-stop jacket is self-terminating when cut.

Typical Application: Mobile phone grounding and interface between aluminum casting and plastic antenna housing.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Compression Set <= 15 %ASTM D3574
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 0.10 ohmCEPS-0002
Shielding Effectiveness 103 dB
@Frequency 1e+9 Hz
 110 dB
@Frequency 1e+8 Hz
 110 dB
@Frequency 1e+10 Hz
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 70.0 °C
Minimum Service Temperature, Air -40.0 °C
 
Descriptive Properties
Adhesive Peel StrengthASTM D1000 (90° Blend)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
General Plastics LAST-A-FOAM® WSF-1010 Foam
BCC Products BC 8870 Polyurethane Elastomer
BCC Products BC 8782 Urethane Casting
BCC Products BC 8675E Polyurethane Elastomer
BCC Products BC 8660E Urethane Elastomer

PCHOME269 / 130979

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.