MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dymax Light Weld® 401 High Clarity Glass Bonding Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes:
Glass Bonding in Seconds
Description

Dymax Light Weld® 400 Series adhesives form high-clarity, invisible bonds between glass and other substrates in seconds. In addition to many structural glass bonding applications, Light Weld 400 Series are excellent, cost effective replacements for optical cements. Adhesives are dishwasher safe, non-yellowing (UV resistant) and exhibit low shrinkage.

Features and Benefits
  • 1 to 60 second cures
  • Solvent-free; no ozone depleting chemicals (O.D.C.s), low V.O.C.s
  • Thermal shock -55°C to 150°C
  • Structural adhesion to 4,000 psi
  • 100% in-line Q.C.
  • Better worker acceptance and low regulatory cost
  • Dishwasher safe
  • Ideal for demanding applications


Dymax 401 Light Weld® High Clarity Glass Bonding Adhesive
Typical Use: Glass furniture; metal brackets to glass, crystal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 90 cPNominal
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85
Tensile Strength, Ultimate 900 psiBond strength to metal
 3700 psiBond strength to glass
Elongation at Break 8.0 %
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.51
Transmission, Visible 90 %clear; thickness not quantified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dymax Ultra Fast™ 3-3095 Tack Gel Adhesive
Resin Technology Group TIGA 142-EX Toughened Epoxy Adhesive
Permabond TA440 Toughened Acrylic Adhesive
Master Bond Supreme 45HTND Toughened Epoxy for Structural Bonding
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives

PDYYMAX05 / 34989

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.