MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Bicor® 84 AOH OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: Bicor AOH is a two-side coating OPP film designed for high oxygen barrier laminations. AOH is designed to be used as the outer web in gas-flush applications for dry products.

Availability: Latin America, North America and South America

Key Features:

  • Excellent optical properties, non-yellowing
  • Good barrier performance
  • Outstanding flavor and aroma barrier
  • PVOH surface is receptive to water-based or solvent based inks and adhesives
  • Requires priming for extrusion laminations
Features:
  • Acrylic Coated
  • Flavor & Aroma Barrier
  • Gas Barrier
  • Oxygen Barrier
  • PVOH Coated
Applications:
  • Crips and Snacks
Uses:
  • VFFS Flexible Packaging
Processing Method: Inner WEb Adhesive Lamination, Out Web Adhesive Lamination, Outer Web Extrusion Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing and Water-based Flexographic Printing

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Vapor Transmission 5.70 g/m²/day
@Temperature 37.8 °C
90% RH
Oxygen Transmission Rate 0.310 cc/m²/day
@Temperature 22.8 °C
0.0% RH; ExxonMobil Method
Thickness 0.840 milNominal; ExxonMobil Method
Coating Weight 12.1 lb/reamExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Coefficient of Friction 0.26Acrylic/Acrylic; ExxonMobil Method
Film Tensile Strength at Break, MD 17500 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 32500 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Haze 1.0 %ExxonMobil Method
Gloss 95 %45º, Acrylic Surface; ExxonMobil Method
 
Descriptive Properties
Yield35600 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Bicor® 85 AXT OPP Film
Ipiranga Petrochem PH 0361 Polypropylene
Ipiranga Petrochem PH 0950 Polypropylene
ExxonMobil Bicor® 420 HS OPP Film
Epsilon Polymers XJ-015 Polypropylene

PEXB377 / 37682

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.