MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Gougeon Brothers Entropy Resins® CPF High Bio-Content, General Purpose Liquid Epoxy Resin
Categories: Polymer; Renewable/Recycled Polymer; Thermoset; Epoxy

Material Notes: High Bio-Content, General Purpose Liquid Epoxy Resin

Product Overview: CPM is a compression molding resin for fast cycle times in heat-assisted molding processes of fiber-reinforced composites. The CPM System delivers a high bio-content, excellent fiber wetting qualities, and thixotropic characteristics to limit sag in high-temperature cure applications. A high modulus combined with excellent elongation properties enable durable yet lightweight composite parts. CPM is a USDA Certified BioPreferred® Product with 30% biobased content

Information provided by Gougeon Brothers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.990 g/cchardener
 1.09 g/ccmixed
 1.13 g/ccresin
Volatile Organic Compounds (VOC) Content 3.31 g/lASTM D2369
Viscosity 1600 cPA
 1700 cPB
 2300 cPMixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 70 - 80
Tensile Strength 8860 psiASTM D638
Elongation at Break 6.0 %ASTM D638
Tensile Modulus 435700 psiASTM D638
Flexural Strength 13560 psiASTM D790
Flexural Modulus 405790 psiASTM D790
Compressive Strength 12630 psiASTM D695
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 159 °FDSC, midpoint
 
Processing PropertiesOriginal ValueComments
Pot Life 20.0 min
 20.0 min
@Temperature >=82.0 °C
 
Descriptive Properties
Mix ratio100:42Weight
 2:1Volume
Mixed Biobased Carbon Content (%)30ASTM D6866

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOUGE984 / 290827

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.