The 54X series gelcoat are formulated with a particular mix of polyester resins, for use in applications where sun exposure and weather conditions are a factor. They are suitable for boats, truck cabs, water slides and environments with humidity and direct sun exposure. This unique formulation is easier and quicker gloss recovery with less buffing time to achieve gloss. Characteristics: - Very good resistance to yellowing and fading due to sun exposure
- Resist to thermal change and weathering
- May be used in submerged application
- Chalking resistant
- Easy to sand and polish