MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Premix Thermoplastics PREADD AS 133
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: PREADD AS 133 is a polyethylene based antistatic masterbatch developed for polyolefines. The active additive in PREADD AS 133 is an amide giving a good antistatic effect already at low dosing levels and at a low humidity. As all migrating antistatic additives PREADD AS 133 may affect the printing, heat sealing and bonding of the film.

The addition level should be tested prior to its use with the polymer used in order to reach the desired antistatic effect. The antistatic effect is dependent on time, humidity and the thickness of the product.

PREADD AS 133 is approved for use in contact with foodstuffs according to FDA and BgVV regulations, as long the dosing level of PREADD AS 133 is less than 10.0%.

Information provided by Premix Thermoplastics Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.920 g/cc
Additive Loading 5.0 %Amide
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 260 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.25 %When Produced
Shelf Life 12.0 MonthNormal Storing Conditions
 
Descriptive Properties
AppearanceGranule
CarrierPE-LD
ColorTransparent
Dosing, %1 to 4Depending on Required Antistatic Effect
 2Standard recommendation for Films and Bottles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPREMA079 / 58094

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.