MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Norplex-Micarta NP515LS Phenolic Glass Laminate Sheet, NEMA G-3
Categories: Polymer; Thermoset; Phenolic

Material Notes: NP515LS is a woven glass fabric combined with a high temperature phenolic resin. It is engineered to provide superior shrink characteristics at elevated temperatures, making it an ideal material for insulating gaskets. Having been tested and certified as a NEMA G-3 material, NP515LS also meets or exceeds the requirements of IEC 60893-3-4 PF GC 201.

Information provided by Norplex-Micarta

Key Words: Glass Fiber, Phenolic, Micarta, NEMA G-3, IEC 60893-3-4 PF GC 201
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.89 g/cc
@Thickness 12.7 mm
ASTM D792
Moisture Absorption 0.560 %
@Thickness 1.57 mm
ASTM D570 Condition A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 112
@Thickness 6.35 mm
ASTM D785
Tensile Strength 54900 psi
@Thickness 3.17 mm
LengthWise; ASTM D638 Condition A
Flexural Strength 49100 psi
@Thickness 1.57 mm
CrossWise; ASTM D790 Condition A
 70200 psi
@Thickness 1.57 mm
LengthWise; ASTM D790 Condition A
Compressive Strength 76400 psi
@Thickness 12.7 mm
Flatwise; ASTM D695 Condition A
Izod Impact, Unnotched 8.50 ft-lb/in
@Thickness 12.7 mm
CrossWise; ASTM D256 Condition E-48/50
 13.7 ft-lb/in
@Thickness 12.7 mm
LengthWise; ASTM D256 Condition E-48/50
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness 1.57 mm
 
Descriptive Properties
Bonding Strength1600[lb]; 0.5"; ASTM D229 Condition D-48/50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elektro-Isola G-Etronax EP S Epoxy, Glass Fabric Reinforcement, Green, Sheets
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet
Norplex-Micarta NP193P Phenolic Aramid Laminate Sheet
Norplex-Micarta NP130 Epoxy Glass Laminate Sheet, NEMA FR-4
Norplex-Micarta MC507U Silicone Glass Laminate Sheet, NEMA G-7

PNORPM063 / 192820

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.