MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Stratasys® Vero™ VERO PUREWHITE RGD837 PolyJet 3D Printing PhotoPolymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Vero is a Rigid Opaque photoPolymer Combination that provides excellent detail visualization and can be blended with other photoPolymer Combinations to vary hardness, flexibility, translucency or heat resistance. 3D print smooth, attractive prototypes to test the fit, form, and function of your static parts, moving components or complex assemblies. Use production systems such as the Stratasys J750 and Connex3 and their multi-material and multi-colour features to produce an impressive range of photorealistic visual effects and lifelike details.

Characteristics

  • Opaque
  • Rigid
  • Dimensionally stable
Options
  • Provide excellent detail visualization
  • 3D print accurate, attractive prototypes that test fit, form and function, even for moving and assembled parts.
  • Produce smooth, accurate jigs, fixtures and manufacturing tooling
Uses
  • Form and fit testing
  • Moving parts and assembled parts
  • Sales, marketing and exhibition models
  • Assembly of electronic components
  • Silicon molding
Advantages
  • Outstanding versatility
  • Fine detail

Information provided by Proto3000

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 - 1.18 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 73.0 - 76.0
Hardness, Shore D 83.0 - 86.0
Tensile Strength 50.0 - 65.0 MPaASTM D-638-03
Elongation at Break 10.0 - 25.0 %ASTM D-638-05
Modulus of Elasticity 2.00 - 3.00 GPaASTM D-638-04
Flexural Strength 75.0 - 110 MPaASTM D-790-03
Flexural Modulus 2200 - 3200 MPaASTM D-790-04
Izod Impact, Notched 20.0 - 30.0 J/mASTM D256-06
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 45.0 - 50.0 °CASTM D648-06
Deflection Temperature at 1.8 MPa (264 psi) 45.0 - 50.0 °CASTM D648-06
Glass Transition Temp, Tg 52.0 - 54.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPROTO827 / 322840

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.