MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
95.5Pd-4.5Ru Alloy, Annealed
Categories: Metal; Nonferrous Metal; Precious Metal; Palladium Alloy

Material Notes: Used for jewelry and electrical contacts.

Key Words: Palladium Ruthenium Alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 12.07 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 147Estimated from Vickers
Hardness, Knoop 171Estimated from Vickers
Hardness, Rockwell A 48Estimated from Vickers
Hardness, Rockwell B 80Estimated from Vickers
Hardness, Vickers 150
Tensile Strength, Ultimate 380 MPa
Elongation at Break 30 %in 5 cm
Modulus of Elasticity 141 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000242 ohm-cmTemperature Coefficient = 0.00032/K (0-100°C)
 
Component Elements PropertiesOriginal ValueComments
Palladium, Pd 95.5 %
Ruthenium, Ru 4.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
95.5Pd-4.5Ru Alloy, Cold Drawn
Overview of materials for Palladium Alloy
77Pd-23Ag Palladium Silver Alloy
75Pd-25Ag Palladium Silver Alloy
70Pd-30Ag Palladium Silver Alloy

MPPdR0 / 12563

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.