PULSE® 959 Engineering resin is a 10% glass reinforced resin designed to provide excellent processability, high heat resistance, and practical toughness. PULSE 959 Engineering resin has been used in automotive interior trim applications. Data provided by Dow Chemical. This product line was spun off from Dow Chemical to Styron in 2010. |