MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Ganpati Exim HA-968 Titanium Dioxide
Categories: Other Engineering Material

Material Notes: HR-968 rutile type titanium dioxide is a kind of pigment made by vitriol method. Zinc oxide is used as its crystal lattice stabilizer. Its surface is treated with inorganic composite consisting of titanium dioxide, silica and a aluminum oxide. It is coated with organic compounds. Coarse powders are removed off in production so that particle size distribution is uniform. The product has excellent luster, outstanding hiding powder, colorability and good dispersibility. Performances of the pigment achieve or surpass that of imported similar products. The pigment is widely used in self-curing paints, some baking finishes, emulsion paints with good luster, textile printing thick liquids, leathers, printing links, laminated cardboards and plastics, (Note: Recommended to use in plastic)

Information provided by Ganpati Exim PVT. LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles >= 0.50 %
@Load 0.100 kg,
Temperature 105 °C
 
Component Elements PropertiesOriginal ValueComments
TiO2 >= 91.5 %
 
Descriptive Properties
Brightness>94
Content>97rutile
Dispersibility (Enterprise Standard)>5
Oil Absorption>23
Solubility>0.5Water Soluble Object
Tint Reducing Power>100compared with the decided standard sample
 >1750compared with standard sample
Value of Aqueous Suspension6.5-9.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGANPATI130 / 317414

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.